Polyester Cord (Class F)

by admin on November 4, 2011

Polyester Cord (Class F)¹

Typical shrinkage 10-11% at 325°F/1hr.
High-tenacity polyester yarn is twisted into a smooth, round, 3-ply construction. It provides improved heat range, added strength and excellent heat shrink characteristics. Increased yield over braided constructions makes it the most economical for high-volume automatic applications. Available on a straight tube or cone-wound.

Suggested Coatings:
“CL” Polyurethane, “W” Wax, “X” Untreated.

 

Part Number Approx. Diameter Inches Nominal Break Lbs. Yield Yds./Lbs. Uncoated Standard Put-Up
DRT-20 .012 16 3260 1 lb.
DRT-30 .016 35 1719 1, 2 lbs.
DRT-45 .026 45 1441 1, 2, 4, 6 lbs.
DRT-50 .028 50 1190 1, 2, 4, 6 lbs.
DRT-65 .030 65 1060 1, 2, 4, 6 lbs.
DRT-100 .040 85 860 1, 2, 4, 6 lbs.
DRT-150 .055 140 405 1, 2, 4 lbs.